I think these are beautiful John, rich tones that seem to glow, love to see the real thing.
Would be great if you could gives us a brief introduction on how you create them
Thank you for appreciation, Martin.
As said, I used the Rockland Tintype Parlor Kit (
https://www.firstcall-photographic.co.uk/rockland-tintype-parlor-kit/p6937) which contains all the necessary chemicals and metal plates to create 8 tintypes on 5x4 size.
I used my Wista N45 and the regular film holders - better use the new plastic ones if you have any, as the old metal type will scratch the plates when loading them. The plates came actually slightly wider (about 2mm) than the holders so I have to trim them using a guillotine (easier to use and more accurate than scissors).
Now, with the plates cut to the right size, under red light I coated them with the provided AG-plus light-sensitive emulsion. That came in a small recipient and is got a solid gel consistency hence I kept it in a jar filled with warm water (aprox. 60C) for about 10 minutes in order to make it liquid. Is a different chemical than the collodion and coating the plates wasn't really a joy. I used my fingers (gloves to be worn) to spread the liquid over the plates' surface. Also I found almost impossible to pour it back into the bottle. I kept a small plastic tray under the plate to collect the excess of liquid (which I reused after warm it up again in hot water). The AG-plus is very sticky and gets back to its initial state quite rapidly so you have to move quickly. This part of the process is the hardest, or I at least found it the hardest.
Once coated, I left the plates to dry in complete darkness, over night, laid on a piece of glass. I read that lean them against a wall for instance is not a good idea as the coating will leak slowly and will become uneven eventualy.
Next day, under the red light again, I loaded my holders and took the shots as explained above.
After exposure, in dark room again, I developed them separately, using approx. 30ml developing solution / each plate, provided in the box. Was about 4-5 minutes for the plates to develop fully. They turn completely black initially then a pale image start to emerge. Once happy with the look, straight from the developer, no rinsing required I dived them in the fixer (provided) for 15mins each. Finally rinse for approx. 15 minutes each in running cold water.
Leave them to dry (I left them over night again). Now I probably have to use a bit of varnish to close the process but I don't have any at the moment so...

Hope that helps and if any questions, please don't be shy.